High saturation magnetic induction to reduce the volume of the iron core;
Rectangular structure---convenient coil assembly;
Iron core opening-excellent resistance to DC bias saturation;
Low loss-reduce temperature rise (1/5-1/10 of silicon steel);
Good stability-can work for a long time at -55-130℃.